Nanoprinted silica glass reaches 5.94 GPa

A 100-micrometer disk of printed resin is heated in air under a microscope. For the first few hundred degrees it does little more than yellow and begin to shrink. At 440 °C it is brown and about 70% of its starting size. Then it clears, becoming transparent again at close to 60% of its original dimensions, and by 1000 °C it has become glass that the team measured at 5.94 GPa in tensile strength. The researchers at the Karlsruhe Institute of Technology (KIT) describe that figure as a record for materials made by two-photon polymerization, a laser-based printing method.
Most heat-based routes to glass still rely on empirical heating schedules, and little was known about how a printed part's internal structure changes during conversion. The KIT team, led by Jiajie Liang, Lisa Hoffmann, Paul Albrecht and Jens Bauer, tracked shrinkage, color, mass loss, mechanics and chemistry side by side, in a study published in Communications Materials. The resin is built around POSS, a silicon-oxygen cage with acrylic groups on its corners. Heating burns off the organic portion and leaves silica. The mechanical path is not a straight line: between 300 and 440 °C, the silica network takes over from the polymer as the main load-bearer, and the part shifts from rubber-like behavior to brittle, with elongation falling to about 9%.
A separate study from the University of California, Irvine, reported in Science, takes a shorter route. Its authors say that optical-grade silica printing has usually required sintering nanoparticles at more than 1,100 °C, while their POSS resin forms a continuous silicon-oxygen network by itself and converts at about 650 °C. A team release relayed by EurekAlert gives calcination shrinkage of about 36%, against about 42% in earlier POSS systems. The two groups do not measure the same things: KIT follows the conversion in detail through its full range, while the Irvine work focuses on removing the sintering step. Earlier work at the University of Freiburg reached fused silica at 600 °C with particle-based resins, and Vilnius University ended with a glass-ceramic at up to 1500 °C.
The numbers have limits. They are measured on micro-scale samples in the laboratory, and the KIT authors tie the dark phase to carbon-rich byproducts. Printed silica also remains less stiff than fused silica, which a related study attributes to residual carbon and molecular-level vacancies. The KIT authors add a condition they call crucial for high-fidelity structures: a self-supporting inorganic network must form before the organic framework breaks down.
Microsystem makers with temperature-sensitive parts could gain, since partial heating gives access to a wide range of stiffness and strength values that the researchers say could suit devices built around components such as conductive aluminum layers. The study gives no date for such use. The authors expect the approach to carry over to other resins and to extend two-photon printing to materials not yet available.