Lab tests: induction heat splits solar mini-modules apart in seconds

At the end of its life, a solar module is hard to open. Two sheets of glass hold a silicon cell, and between them sits a plastic layer of ethylene vinyl acetate (EVA) that glues everything together. A team from the Korea Electronics Technology Institute (KETI) in South Korea and the University of New South Wales (UNSW) in Australia has found a way to separate those layers in seconds. In the team's fastest test, the layers came apart in 5 seconds, and the cell came out intact, with no visible polymer residue on its surface.
The key is induction heating. A water-cooled copper coil heats the metal contacts on the cell, which decomposes the EVA locally, at the interface with the cell, while the glass stays cooler. Tests showed a temperature gap of more than 200 °C between cell and glass at a coil current of 100 A. The samples hang with the cell facing down, so gravity helps it drop away: on a 2 cm × 2 cm sample, separation took about 14 seconds. Another route, pyrolysis above 500 °C, described in one study, removes more than 99% of the EVA and frees the glass but gets rid of the glue as well. Here, spectroscopy shows that the remaining EVA largely keeps its chemical structure.
The team then built glass-glass mini-modules, each with one passivated emitter and rear contact (PERC) cell, a type of silicon cell, EVA, and two sheets of tempered glass, 5 cm × 8 cm and 1 mm thick. Gases released by the heated EVA need a way out, so release films of polytetrafluoroethylene (PTFE), each with a 1.8 cm × 1.8 cm opening, were placed on both sides of the cell. The coil current set the pace: 18.6 seconds at 100 A, 8.3 seconds at 150 A and 5.4 seconds at 200 A. Taiyangnews, which also covered the study, points out that the glass-glass design makes it harder for those gases to escape, which is the problem the release films address. The mini-modules gave back 99.8% of their total mass, with negligible losses of glass, cells and films.
The figures are the team's own, from its paper in Communications Materials, and the samples remain small: a single cell in a 5 cm × 8 cm mini-module, not a full panel. Mechanical scraping of the EVA off the glass afterwards caused a loss of less than 10% of the encapsulant's mass, and microscopy found no significant residue or structural damage on the recovered cells. Full-size commercial panels have not yet been tested.
For recyclers, the gain is speed and cleaner material: glass, cell and film come out separately, and the cell comes out clean. That gain applies to small samples for now. Lee says the next step is to apply the process to full-size commercial PV panels and scale it up for commercial recycling operations, but the researchers give no date for it, and no cost estimate.
Sources — read the originals(Paris time)